Im sorry our aluminum suplier told us 6063 grade was as stong as 6061, we liked the rounded edge, but when we foud out this was not as strong, we changed back to 6061t6 and aded a doubler reenforcment strip so far tested for 2 months, this mistake i admit to and has cost me alot, the new ones are better way way better